header advert
You currently have no access to view or download this content. Please log in with your institutional or personal account if you should have access to through either of these
The Bone & Joint Journal Logo

Receive monthly Table of Contents alerts from The Bone & Joint Journal

Comprehensive article alerts can be set up and managed through your account settings

View my account settings

Get Access locked padlock

Hip

Differences in ion release after ceramic-on-ceramic and metal-on-metal total hip replacement

MEDIUM-TERM FOLLOW-UP



Download PDF

Abstract

Modern metal-on-metal bearings produce less wear debris and osteolysis, but have the potential adverse effect of release of ions. Improved ceramic-on-ceramic bearings have the lowest wear of all, but the corrosion process has not been analysed.

Our aim was to measure the serum ion release (ng/ml) in 23 patients having stable hip prostheses with a ceramic-on-ceramic coupling (group A) and to compare it with the release in 42 patients with a metal-on-metal bearing (group B) in the medium term. Reference values were obtained from a population of 47 healthy subjects (group C). The concentrations of chromium, cobalt, aluminium and titanium were measured.

There was a significant increase of cobalt, chromium and aluminium levels (p < 0.05) in group B compared with groups A and C. Group A did not differ significantly from the control group. Despite the apparent advantage of a metal-on-metal coupling, especially in younger patients with a long life expectancy, a major concern arises regarding the extent and duration of ion exposure. For this reason, the low corrosion level in a ceramic-on-ceramic coupling could be advantageous.